150 Most Recent Posts

Thread AuthorPostersPost AuthorForumThread/Post Link
Bill J. from Austin2Papa ZookHarley Freewheeler /...16" front rim?
ZZMACH11ZZMACH1Harley Tri GlideLooking for Dynajet Power Vision mo...
Bill J. from Austin2Bill J. from AustinHarley Freewheeler /...16" front rim?
HDUSA17cycle7447New Member Introduct...New to Trike Talk
HDUSA17hardwickbvNew Member Introduct...New to Trike Talk
ZZMACH11ZZMACH1Harley Tri GlideNew Member Hello from NH
ZZMACH11ZZMACH1Harley Tri GlideElectric Fans on 2014 Tri Glide
MDO100JTJerseyHarley Freewheeler /...What Did You Do To Your Freewheeler...
chucktrue558My TurnHarley Freewheeler /...Rear shock adjustment
HDUSA17trike ladyNew Member Introduct...New to Trike Talk
HDUSA12cycle7447Harley Trike Convers...Harley TPMS sensor and aftermarket ...
HDUSA12HDUSA1Harley Trike Convers...Harley TPMS sensor and aftermarket ...
HDUSA12cycle7447Harley Trike Convers...Harley TPMS sensor and aftermarket ...
HDUSA17SullyNew Member Introduct...New to Trike Talk
HDUSA12HDUSA1Harley Trike Convers...Harley TPMS sensor and aftermarket ...
Bonsai13woodyNew Member Introduct...New member from Texas
HDUSA17woodyNew Member Introduct...New to Trike Talk
HDUSA17rhino 2New Member Introduct...New to Trike Talk
HDUSA17HDUSA1New Member Introduct...New to Trike Talk
chucktrue558Old Road DogHarley Freewheeler /...Rear shock adjustment
stancotreau3stancotreauLehman TrikeLehman Storm rear brake pads
Tritek2trike ladyLehman TrikeAvoid buying a Lehman?
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
Bonsai13hardwickbvNew Member Introduct...New member from Texas
Davep12hardwickbvNew Member Introduct...Hello from the mountains
LD-Ordie11hardwickbvNew Member Introduct...Newbie from the Mojave Desert
ZZMACH14ZZMACH1Harley Tri GlideElectric Fans on 2014 Tri Glide
ctdair9ROAD DOGHarley Tri GlideHot Rotors After New Pads
Zammy1ZammyGeneral DiscussionHappy Birthday "prariepilot&qu...
Sunman7BowdenTrikeHonda TrikesF1 Warning Light
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
Jack Klarich3Jack KlarichGeneral DiscussionMY first guitar
hardwickbv4ctdairHarley Tri GlideGot a Code P0152 Engine Running Ric...
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
woody13Rogue1Maggie Valley Gather...Maggie Valley 2024
Davep12PosseRiderNew Member Introduct...Hello from the mountains
chucktrue558Jack KlarichHarley Freewheeler /...Rear shock adjustment
ZZMACH12Jack KlarichHarley Tri GlideSTOCK HARLEY ECM MAP with DynoJet
ctdair9Jack KlarichHarley Tri GlideHot Rotors After New Pads
rhino 212Jack KlarichGeneral DiscussionRainey day thought's ¶¶¶
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
rhino 212rhino 2General DiscussionRainey day thought's ¶¶¶
ZZMACH12ZZMACH1Harley Tri GlideSTOCK HARLEY ECM MAP with DynoJet
ctdair9ROAD DOGHarley Tri GlideHot Rotors After New Pads
rhino 2121dn5upGeneral DiscussionRainey day thought's ¶¶¶
ZZMACH14ZZMACH1Harley Tri GlideElectric Fans on 2014 Tri Glide
Davep12SullyNew Member Introduct...Hello from the mountains
rhino 212Phu CatGeneral DiscussionRainey day thought's ¶¶¶
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
ZZMACH14ol' schoolHarley Tri GlideElectric Fans on 2014 Tri Glide
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
hardwickbv4KoolbreezeHarley Tri GlideGot a Code P0152 Engine Running Ric...
Davep12DavepNew Member Introduct...Hello from the mountains
Davep12woodyNew Member Introduct...Hello from the mountains
rhino 212rhino 2General DiscussionRainey day thought's ¶¶¶
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
dthorn6Jack KlarichHarley Tri Glide2024 Tri Glide front axle nut torqu...
rhino 212Jack KlarichGeneral DiscussionRainey day thought's ¶¶¶
ctdair9Jack KlarichHarley Tri GlideHot Rotors After New Pads
rhino 2121dn5upGeneral DiscussionRainey day thought's ¶¶¶
Davep12Jack KlarichNew Member Introduct...Hello from the mountains
Davep12ol' schoolNew Member Introduct...Hello from the mountains
Tritek2TritekLehman TrikeAvoid buying a Lehman?
ZZMACH14Rmitchell55Harley Tri GlideElectric Fans on 2014 Tri Glide
Davep12trike ladyNew Member Introduct...Hello from the mountains
Bonsai13Marc HNew Member Introduct...New member from Texas
Davep12Marc HNew Member Introduct...Hello from the mountains
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
woody13PosseRiderMaggie Valley Gather...Maggie Valley 2024
Bonsai13ZammyNew Member Introduct...New member from Texas
woody13PosseRiderMaggie Valley Gather...Maggie Valley 2024
Davep12ZammyNew Member Introduct...Hello from the mountains
chucktrue558ZammyHarley Freewheeler /...Rear shock adjustment
Bonsai13Uncle FesterNew Member Introduct...New member from Texas
Davep12Uncle FesterNew Member Introduct...Hello from the mountains
ZZMACH14rhino 2Harley Tri GlideElectric Fans on 2014 Tri Glide
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
dthorn6dthornHarley Tri Glide2024 Tri Glide front axle nut torqu...
ZZMACH14ZZMACH1Harley Tri GlideElectric Fans on 2014 Tri Glide
ctdair9MykneesbehurtinHarley Tri GlideHot Rotors After New Pads
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
chucktrue558rhino 2Harley Freewheeler /...Rear shock adjustment
chucktrue558JTJerseyHarley Freewheeler /...Rear shock adjustment
chucktrue558ROAD DOGHarley Freewheeler /...Rear shock adjustment
ctdair914TGHarley Tri GlideHot Rotors After New Pads
Sunman7pwhoeverHonda TrikesF1 Warning Light
Sunman7pwhoeverHonda TrikesF1 Warning Light
Davep6DavepHarley Tri GlideTRI GLIDE AIR FILTER QUESTION
Sunman7GoldWingrGregHonda TrikesF1 Warning Light
chucktrue558chucktrue55Harley Freewheeler /...Rear shock adjustment
chucktrue558rhino 2Harley Freewheeler /...Rear shock adjustment
Davep12rhino 2New Member Introduct...Hello from the mountains
Davep12DavepNew Member Introduct...Hello from the mountains
chucktrue558chucktrue55Harley Freewheeler /...Rear shock adjustment
Bonsai13Papa ZookNew Member Introduct...New member from Texas
Bonsai13SullyNew Member Introduct...New member from Texas
Bonsai13BonsaiNew Member Introduct...New member from Texas
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
ctdair9Jd1aHarley Tri GlideHot Rotors After New Pads
hardwickbv4Jack KlarichHarley Tri GlideGot a Code P0152 Engine Running Ric...
DrCrazyTrain5Jack KlarichHarley Freewheeler /...True Dual Header
Bonsai13Jack KlarichNew Member Introduct...New member from Texas
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
Jack Klarich3Jack KlarichGeneral Harley ChatExhaust Heat Shield
gfaltersack8Jack KlarichHarley Tri GlideDK Customs remote oil filter kit in...
kj5ix32ADSavareseHonda TrikesMotor Trike Service Manual Finished
gfaltersack8Old Road DogHarley Tri GlideDK Customs remote oil filter kit in...
Davep6Old Road DogHarley Tri GlideTRI GLIDE AIR FILTER QUESTION
ctdair9Old Road DogHarley Tri GlideHot Rotors After New Pads
Bonsai13ol' schoolNew Member Introduct...New member from Texas
Sunman7rhino 2Honda TrikesF1 Warning Light
Papa Zook1Papa ZookHarley Tri Glide2024 Harley Trikes Lineup - Laidlaw...
Bonsai13rhino 2New Member Introduct...New member from Texas
Bonsai13GorillaNew Member Introduct...New member from Texas
Rawhideken1714TGHarley Tri Glide2024 Tri glide
kj5ix32trike ladyHonda TrikesMotor Trike Service Manual Finished
Bonsai13trike ladyNew Member Introduct...New member from Texas
Bonsai13BonsaiNew Member Introduct...New member from Texas
Sunman7BowdenTrikeHonda TrikesF1 Warning Light
LD-Ordie11Marc HNew Member Introduct...Newbie from the Mojave Desert
DK Custom Products362ZammyHarley Tri GlideWhat did you do to Your Tri-Glide T...
ADSavarese13ZammyNew Member Introduct...New member from FL
DrCrazyTrain5rhino 2Harley Freewheeler /...True Dual Header
DK Custom Products362rhino 2Harley Tri GlideWhat did you do to Your Tri-Glide T...
ctdair9ctdairHarley Tri GlideHot Rotors After New Pads
LD-Ordie11ZammyNew Member Introduct...Newbie from the Mojave Desert
LD-Ordie11Uncle FesterNew Member Introduct...Newbie from the Mojave Desert
DrCrazyTrain5Ron BaxterHarley Freewheeler /...True Dual Header
Burnerboy10rhino 2Can Am Spyder Trike...How many of you ride a Can Am spyde...
DK Custom Products362PosseRiderHarley Tri GlideWhat did you do to Your Tri-Glide T...
Davep6rhino 2Harley Tri GlideTRI GLIDE AIR FILTER QUESTION
Sunman8PuckoachHarley Freewheeler /...Value of 2015 Freewheeler
dthorn6rhino 2Harley Tri Glide2024 Tri Glide front axle nut torqu...
gfaltersack8rhino 2Harley Tri GlideDK Customs remote oil filter kit in...
gfaltersack8gfaltersackHarley Tri GlideDK Customs remote oil filter kit in...
hardwickbv4hardwickbvHarley Tri GlideGot a Code P0152 Engine Running Ric...
dthorn6dthornHarley Tri Glide2024 Tri Glide front axle nut torqu...
dthorn6Papa ZookHarley Tri Glide2024 Tri Glide front axle nut torqu...
dthorn6dthornHarley Tri Glide2024 Tri Glide front axle nut torqu...
SSpoon14cycle7447New Member Introduct...Hello from VA
Richard D12CorkeykHarley Trike Convers..."Himsl Praying Mantis" Sh...
gfaltersack8ISP-FLHarley Tri GlideDK Customs remote oil filter kit in...
gfaltersack8gfaltersackHarley Tri GlideDK Customs remote oil filter kit in...
Cut N Shoot Customs2miaboboCut N Shoot CustomsGL1800 & GL1500 Fork Tube Exten...
LD-Ordie11ol' schoolNew Member Introduct...Newbie from the Mojave Desert
Rawhideken17KoolbreezeHarley Tri Glide2024 Tri glide
LD-Ordie11trike ladyNew Member Introduct...Newbie from the Mojave Desert
Davep6KoolbreezeHarley Tri GlideTRI GLIDE AIR FILTER QUESTION
Davep6DavepHarley Tri GlideTRI GLIDE AIR FILTER QUESTION
myhonda614TGHarley Tri GlideKuryakyn filler pad
Likes Likes:  3
Thanks Thanks:  1
Results 1 to 20 of 20

Thread: 2013 Victory Vision Crossbow frame weld cracked

  1. #1
    5+ Posts
    Join Date
    Dec 2020
    Location
    Philadelphia, PA USA
    Posts
    7

    Default 2013 Victory Vision Crossbow frame weld cracked

    Hit a speed bump and right side of trike collapsed into wheel well due to weld breaking at right side crossmember to wheel arm and broke belt in the process of getting it off the road. Now I have a broken obsolete trike that I can't seem to find parts for ( trike kit parts) and nobody wants to touch it (as far as welding) due to liability issues. Coming here to get some ideas and suggestions as I am at a loss as what to do. It was fully covered and insurance company adjuster wrote an $1200. estimate which I didn't accept due to reasons above... Help! 🙃
    2013 Victory Vision Tour Crossbow Trike in Black, Miller Mufflers, Trailer Hitch w/ Bushtec lock pin.
    ********* No Good Deed Goes Unpunished *********

  2. #2
    800+ Posts
    Gold Club Member

    Join Date
    Nov 2021
    Location
    Lake Orion, MI, USA
    Posts
    805

    Default

    Quote Originally Posted by Cruiser5406 View Post
    Hit a speed bump and right side of trike collapsed into wheel well due to weld breaking at right side crossmember to wheel arm and broke belt in the process of getting it off the road. Now I have a broken obsolete trike that I can't seem to find parts for ( trike kit parts) and nobody wants to touch it (as far as welding) due to liability issues. Coming here to get some ideas and suggestions as I am at a loss as what to do. It was fully covered and insurance company adjuster wrote an $1200. estimate which I didn't accept due to reasons above... Help! 🙃
    Try this - since the adjuster wrote a $1200 estimate, he must have gotten that figure from somewhere? Perhaps he can provide his supplier's contact info and they can fix it. If not, then maybe they will total it.

  3. #3
    99500 + Posts
    Gold Club Member
    rhino 2's Avatar
    Join Date
    Oct 2011
    Location
    Utopia New Jersey USA..
    Posts
    99,965

    Default

    Have you tried talking with the shop that installed the trike kit….I see you’re from Philly… hopefully it wasn’t from new Berlin New Jersey..I think they close shop..?
    Sometimes a Cigar is Just a Cigar.....
    2019 Tri-Glide.......

  4. #4
    18000+ Posts
    Tech Contributor
    Gold Club Member
    Jack Klarich's Avatar
    Join Date
    Oct 2016
    Location
    Jax, Fla USA
    Posts
    18,269

    Default

    First thing to find out, if you keep it and have it welded does it need to be certified by your state?
    Nuff Said," Were Burnin Daylight, Lets Ride"(Sober 37 years)
    Current ride : 2021 FREEWHEELER M8, oldest ride 1960 FL

  5. #5
    Contributing Member ROAD DOG's Avatar
    Join Date
    Jan 2009
    Location
    MA,
    Posts
    1,006

    Default

    Is it steel or aluminum? The insurance adjuster more than likely pulled that number out of his Ass ! he has no books or anything to go by on the parts time or labor. Can you post a picture ? Find a good Welder have them weld it up & reinforce it , if the weld broke it can be rewelded & made better than new . I dont see a big deal .

  6. #6
    100+ Posts
    Join Date
    Feb 2017
    Location
    DE
    Posts
    126

    Default

    Street rod frame builder, would be your best bet, send pics, or talk to s&w in spring city pa.

  7. #7
    99500 + Posts
    Gold Club Member
    rhino 2's Avatar
    Join Date
    Oct 2011
    Location
    Utopia New Jersey USA..
    Posts
    99,965

    Default

    Quote Originally Posted by ROAD DOG View Post
    Is it steel or aluminum? .
    The victory, crossbow bikes are aluminum frame..
    Sometimes a Cigar is Just a Cigar.....
    2019 Tri-Glide.......

  8. #8
    100+ Posts
    Join Date
    Feb 2017
    Location
    DE
    Posts
    126

    Default

    Also, a big warning out, to all the others to check your frames. Victory or otherwise with same kit

  9. #9
    5+ Posts
    Join Date
    Dec 2020
    Location
    Philadelphia, PA USA
    Posts
    7

    Default

    Quote Originally Posted by rhino 2 View Post
    The victory, crossbow bikes are aluminum frame..
    The part that is cracked would be like a sub frame for the trike part only. It connects the bike to the trike part. It is steel. I will try to post pic as it has part # or serial number on it.

  10. #10
    5+ Posts
    Join Date
    Dec 2020
    Location
    Philadelphia, PA USA
    Posts
    7

    Default

    This is the factory Crossbow kit that was installed only in Spearfish, SD by Lehman. The Vision is Aluminum frame bike however the trike kit and most parts are steel.
    2013 Victory Vision Tour Crossbow Trike in Black, Miller Mufflers, Trailer Hitch w/ Bushtec lock pin.
    ********* No Good Deed Goes Unpunished *********

  11. #11
    99500 + Posts
    Gold Club Member
    rhino 2's Avatar
    Join Date
    Oct 2011
    Location
    Utopia New Jersey USA..
    Posts
    99,965

    Default

    Quote Originally Posted by Cruiser5406 View Post
    The part that is cracked would be like a sub frame for the trike part only. It connects the bike to the trike part. It is steel. I will try to post pic as it has part # or serial number on it.
    Who made/ manufactured the Trike part …And did you install it yourself?..Or did you have it done by a shop?
    Sometimes a Cigar is Just a Cigar.....
    2019 Tri-Glide.......

  12. #12
    100+ Posts
    Join Date
    Feb 2017
    Location
    DE
    Posts
    126

    Default

    Tried to dm you, is part removable, ect. Try n message me.

  13. #13
    5250+ Posts Pegasus1300's Avatar
    Join Date
    Oct 2011
    Location
    Spring City,Utah, USA
    Posts
    5,299

    Default

    Find a fabricator or frame builder there in the Northeast. See if he will build you some fish plates to connect the trike (steel)to the Victory frame (aluminium ) without welding. Do both sides. You will probably have to travel a bit. I am assuming you have tried to contact the old Lehman shop or their successors, if any? I thought one of the major trike companies took on the shop.
    Happy TRAils/NSD
    Paul

  14. #14
    5+ Posts
    Join Date
    Dec 2020
    Location
    Philadelphia, PA USA
    Posts
    7

    Default

    Quote Originally Posted by rhino 2 View Post
    Who made/ manufactured the Trike part …And did you install it yourself?..Or did you have it done by a shop?
    This was / is a Factory (Lehman) made Crossbow trike kit installed at Lehman facility in Spearfish , SD . I bought it used already built in 2018 on consignment for $20K at the original shop that sent this bike to be built into trike back in 2013. I believe the axle is made by Champion? The rest of trike kit was made and built exclusively by Lehman. This is best info I have learned but all parties involved seem to be no longer in business.
    2013 Victory Vision Tour Crossbow Trike in Black, Miller Mufflers, Trailer Hitch w/ Bushtec lock pin.
    ********* No Good Deed Goes Unpunished *********

  15. #15
    5+ Posts
    Join Date
    Dec 2020
    Location
    Philadelphia, PA USA
    Posts
    7

    Default

    Quote Originally Posted by TwistedKarma View Post
    Tried to dm you, is part removable, ect. Try n message me.
    I am going to try to disassemble the trike and remove that part and see if it can be fixed or maybe fabricate a new one but seriously, I would love to find a way to put an Independent suspension on this trike as the ride is awesome on nice roads but where I live in Phila, PA , it's annoying and painful. It's called live and learn I guess. I just want to ride the damn thing and I have the worse luck with decision making and choices I usually regret. Still Victory is my favorite and zero regrets on the bike part ever!
    2013 Victory Vision Tour Crossbow Trike in Black, Miller Mufflers, Trailer Hitch w/ Bushtec lock pin.
    ********* No Good Deed Goes Unpunished *********

  16. #16
    99500 + Posts
    Gold Club Member
    rhino 2's Avatar
    Join Date
    Oct 2011
    Location
    Utopia New Jersey USA..
    Posts
    99,965

    Default

    Quote Originally Posted by Cruiser5406 View Post
    I am going to try to disassemble the trike and remove that part and see if it can be fixed or maybe fabricate a new one but seriously, I would love to find a way to put an Independent suspension on this trike as the ride is awesome on nice roads but where I live in Phila, PA , it's annoying and painful. It's called live and learn I guess. I just want to ride the damn thing and I have the worse luck with decision making and choices I usually regret. Still Victory is my favorite and zero regrets on the bike part ever!
    Victory a.k.a. Polaris made a great bike. I had one of the iron frame ones the gunner’ but as soon as Polaris pulled the plug on Victory, I traded it in for another triglide…
    Sometimes a Cigar is Just a Cigar.....
    2019 Tri-Glide.......

  17. #17
    850+ Posts Rmitchell55's Avatar
    Join Date
    Dec 2012
    Location
    Santee
    Posts
    894

    Default

    Lehman trikes was bought out by Champion when John Lehman died, the Champion was bought by D & D Cycles in Mesa, AZ. ?? I don't know if Champion of AZ. still has parts for Lehman.
    Ray
    2017 Harley Triglide
    Tijuana Border

  18. #18
    5+ Posts
    Join Date
    Jan 2019
    Location
    Lenexa, ks
    Posts
    8

    Default

    This happened to my 2011 Vision trike. The original owner was a millwright. I believe he took off the fenders and found the broken welds. He then made some gussets or brackets and welded them where the were cracked or broken making them stronger then they were. My question is now how to lift up the trike to inspect the under carriage that he welded. Any help there??

  19. #19
    100+ Posts
    Join Date
    Feb 2017
    Location
    DE
    Posts
    126

    Default

    Ramps for a car? 2x8. With bracing slower incline, could that help?

  20. #20
    30+ Posts
    Join Date
    Mar 2023
    Location
    Bellmawr
    Posts
    30

    Default

    Quote Originally Posted by rhino 2 View Post
    Have you tried talking with the shop that installed the trike kit….I see you’re from Philly… hopefully it wasn’t from new Berlin New Jersey..I think they close shop..?
    The Trike Shop that was in Berlin, NJ (Ace Trike) moved to Glassboro for a few years. As of last October they moved again, this time to Harrington, DE.

Similar Threads

  1. Replies: 3
    Last Post: 07-25-2021, 06:35 AM
  2. NEED HELP!... What Angle to Weld New Neck Tube onto my Frame????
    By inkslingersourwine in forum VW Powered Trikes
    Replies: 9
    Last Post: 02-18-2017, 06:40 PM
  3. Lehman Trikes CrossBow now available for 2014 Victory Vision!
    By Trike Talk News in forum Victory Trikes
    Replies: 2
    Last Post: 05-21-2014, 02:55 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •